Soft soldering in electronics

Soft soldering joins components and circuit board with a molten solder whose melting temperature is below 450 °C, without melting the parts themselves. In electronics the solder is a tin alloy; the flux removes oxides and ensures wetting.

Explanation

In through-hole (THT) soldering the component lead is inserted through the hole in the board. The tip heats pad and lead at the same time; then solder is fed to the joint, not to the tip. It flows around the lead once both are hot enough. After a short dwell, first the solder and then the iron are removed, and the joint must not move while it solidifies.

A good joint is smooth, has a concave fillet and fully wets pad and lead. Lead-free solders, mandatory in the EU for most electrical equipment, melt at higher temperatures than the tin-lead solders used earlier and look somewhat duller. Typical faults are cold joints, solder bridges between adjacent pins and lifted pads from too much heat or too long a dwell.

Many integrated circuits are sensitive to electrostatic discharge. Soldering is therefore done at an earthed workstation, and components are taken out of their protective packaging only when they are inserted. Solder fumes are extracted.

Guide value; follow the manufacturer’s data.

In practice: Design & Make – Mecanum rover, Circuit board (motor driver board)

On the fourth day of the Design & Make workshop participants design the rover's motor driver board and solder it together: two L293D in DIP-16 packages, 2.54 mm pitch, four motor outputs. In the video the tip temperature is about 410 °C (in practice often 330 to 380 °C, follow the manufacturer’s data), with roughly one to two seconds of dwell after feeding the solder. The project data name the cold joint as the most common fault, because it is missed in the visual check and only fails sporadically later.

To the training project Design & Make – Mecanum rover

Common mistakes

  • Feeding solder to the tip instead of the joint. The flux burns off before it can act.
  • Moving the joint while it solidifies. The result is a cold joint with intermittent contact.
  • Soldering too long or too hot. The pad lifts off the board.
  • Inserting the IC the wrong way round. Pin 1 is to the left of the notch.