Explanation
Wrought aluminium alloys are designated EN AW plus a four-digit number. The first digit names the main alloying element: 1xxx pure aluminium, 2xxx copper, 3xxx manganese, 4xxx silicon, 5xxx magnesium, 6xxx magnesium and silicon, 7xxx zinc. There is also the chemical designation, e.g. AlMg3 for 5754. Older documents still use names like AlMgSi0.5, which is today's 6060.
5xxx alloys are not strengthened by heat treatment but by cold working. Their temper is given with H and digits. They bend and weld well and resist damp and salty environments. 6xxx alloys are hardened by solution treatment, quenching and ageing; the temper is stated with T and digits, e.g. T6. 6060 has medium strength and a very good surface; the related 6061 is stronger and popular for milled parts.
When machined, aluminium tends to form built-up edges. Sharp tools with a large rake angle, high cutting speed and coolant help. Bending age-hardened alloys requires larger radii than mild steel sheet.
In practice: Buggy, Engine block
For the buggy's engine block the project data recommend a free-machining alloy such as AlMgSi0.5 (today EN AW-6060) or AlCuMgPb, with 75 × 55 × 28 mm flat stock as the blank. The chassis and rims of the mechanical race car are EN AW-6061 (AlMg1SiCu); the chassis is milled from a 258 × 80 × 56 mm block. In both projects the data warn of smeared surfaces caused by built-up edges.
Common mistakes
- Ordering "aluminium" without alloy and temper. Strength, machinability and bendability differ greatly.
- Bending an age-hardened 6xxx alloy with a small radius. It cracks on the outside.
- Using steel tools and cutting data in aluminium. The result is built-up edges and poor surfaces.