Explanation
A slicer divides the model, usually a mesh (STL or 3MF), into layers and calculates the nozzle paths. The key settings: layer height, number of wall lines (perimeters), infill percentage and pattern, nozzle and bed temperatures, and supports. Layer height determines surface and print time; it stays well below the nozzle diameter, with 0.2 mm common for a 0.4 mm nozzle.
Printed parts are not equally strong in all directions: bonding between layers is weaker. Orientation in the build space therefore helps determine strength. Overhangs up to about 45° usually print without support; flatter ones need support. Holes often come out slightly smaller than designed, the first layer can spread (elephant's foot), and large flat parts warp as they cool. Where dimensions matter, a manufacturing model with print allowance or a test print helps.
Formulas and worked example
Given: Part 5 mm high, layer height 0.2 mm
Guide value; follow the manufacturer’s data.
In practice: Design & Make – Mecanum rover, Roof (housing cover)
Almost all plastic parts of the Mecanum rover are made by FDM printing. For the housing cover the project data give guide values for PLA: nozzle 200 to 215 °C, bed 55 to 60 °C, layer height 0.2 mm with a 0.4 mm nozzle, and with a 3 mm wall three to four perimeters and 15 to 20 % infill. Corner chamfers and draft angles make it printable without support. On the race car the front and rear spoilers are printed; there the topics are part orientation, hole compensation and the 45° rule.
To the training project Design & Make – Mecanum rover
Common mistakes
- Orienting a part so that the main load acts across the layers. It breaks along a layer line.
- Printing fitted holes at nominal size and expecting them to fit. They usually come out smaller.
- Modelling threads only cosmetically. They are missing from the mesh and a smooth cylinder gets printed.